ASTM D3826

Standard Practice for Determining Degradation End Point in Degradable Polyethylene and Polypropylene Using a Tensile Test
The Standard covers a degradation end point or a brittle point, for degradable polyethylene / polypropylene films and sheets less than 1.0 mm thick. The tensile elongation property can be used to provide data for research and development and engineering design, as well as quality control specifications.